TY - JOUR
AU - Oliveira, J. P.
AU - Fernandes, F. M. Braz
AU - Schell, N.
AU - Miranda, R. M.
TI - Martensite stabilization during superelastic cycling of laser welded NiTi plates
JO - Materials letters
VL - 171
SN - 0167-577X
CY - New York, NY [u.a.]
PB - Elsevier
M1 - PUBDB-2016-01212
SP - 273 - 276
PY - 2016
N1 - (c) Elsevier B.V.
AB - Superelastic behavior of laser welded NiTi is significantly different from the original base material due tomicrostructural changes introduced during welding. These are responsible for a higher accumulated irrecoverablestrain during mechanical cycling. In order to clarify the mechanisms responsible for theevolution of the accumulated irrecoverable strain on superelastic laser welded NiTi, detailed synchrotronX-ray diffraction analysis was performed. Welded samples were analyzed as-welded, after 4 cycles at 10
LB - PUB:(DE-HGF)16
UR - <Go to ISI:>//WOS:000372156200067
DO - DOI:10.1016/j.matlet.2016.02.107
UR - https://bib-pubdb1.desy.de/record/295890
ER -